By Barry Marsh - 7/22/2020 9:56:38 PM
Hi,
Was wondering if anybody has any good suggestions to alternatives to carbon fiber and resin for testing setups. So that I am not wasting as much carbon and resin I am looking for a way to do a dry run.
I had thought maybe some kind of cheap material and a liquid that has a similar viscosity to the IN2 resin that EC sells.
I understand that the only real way to test is with the real materials but wonder if there would be any value in doing a test like this and if anybody on here does this?
Thanks for any input / ideas
|
By Barry Marsh - 7/23/2020 9:11:07 PM
Yeah thanks again the the extra suggestion there. I didn’t so much need anything that would set, but just to get an idea about the flow while it’s live.
|
|