Infusion with IN2 Epoxy and GC50 Epoxy Polyester Gelcoat


Author
Message
ahender
a
Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)
Group: Forum Members
Posts: 38, Visits: 300
Is this correct?

Roll my mold with GC50 gel coat, wait a few hours till it is tacky but will not adhere to finger, add the reinforcement and infuse with IN2 epoxy.

Thanks...Alan


Replies
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
If you're referring to GC50 itself, you can only apply a single coat, as it won't bond well to itself, unlike conventional polyester gel coatings (which shouldn't be used to make epoxy parts)

Once applied, it can be left up to 24hrs and still bond okay to the epoxy. I have, on very rare occasions, left it a little longer and things appeared to be alright. Ideally, though, it is usually ready to go after a couple of hours at reasonable ambient temperatures. 


ahender
a
Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)
Group: Forum Members
Posts: 38, Visits: 300
MarkMK - 7/13/2020 7:56:10 AM
If you're referring to GC50 itself, you can only apply a single coat, as it won't bond well to itself, unlike conventional polyester gel coatings (which shouldn't be used to make epoxy parts)

Once applied, it can be left up to 24hrs and still bond okay to the epoxy. I have, on very rare occasions, left it a little longer and things appeared to be alright. Ideally, though, it is usually ready to go after a couple of hours at reasonable ambient temperatures. 


Thank you very much for answering my questions. At a recommendation of approximately 
.5 mm to .7 mm in thickness, it seems this would be impossible to do using a roller. I am not set up to spray the gel coat. 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ahender - 5 Years Ago
MarkMK - 5 Years Ago
ahender - 5 Years Ago
MarkMK - 5 Years Ago
ahender - 5 Years Ago
Warren (Staff) - 5 Years Ago
ahender - 5 Years Ago
Warren (Staff) - 5 Years Ago
ahender - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you.
ahender - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search