First Attempt


Author
Message
MaxiDave
MaxiDave
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 158
Not sure if this is the correct section so please move if need be.

Up until last week I never even held a piece of carbon or kevlar cloth

until I undertook this massive project.

The plan is to make a complete wide arch bodykit for a 106 Maxi rally car and it had

to be kevlar as per the genuine Peugeot sport item.

I sourced a set of moulds, got all my material from Easy Composites and jumped in feet first.

I did it all hand lay up, 1 layer of 300g kevlar, 2 diolen and a final 300g kevlar.

I'm more than delighted with the results, a few dry spots but its going to be painted anyway so I can fill the low spots.














Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Very Nice!!!!
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
looks good! is it stiff enough?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Leon
Leon
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 59, Visits: 606
Hii.. 

That would be Looks great and cost effectiveness for painted product finish, kevlar is dificult enough to trim and cut.. realy great for abrasion purpose. What the resin you use for hand lay up  this fabric?

Regards

Leon
MaxiDave
MaxiDave
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 158
I was able to stand on the wing without doing any damage.

The quarter panels are a little more flexable so I might add some kevlar

square patches to the rear for more stiffness. I have already used 5-6 layers of kevlar

around the wheel arch area to add strength incase it rubs the wheel or is

lifted by the arch. 
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
Those panels looks great and really impressive given you have just started doing this - great find getting hold of the moulds!
Have you looked at the carbon/kevlar mixes? eg Carbon/Twaron
I've got some of this sat waiting for some Lotus Sunbeam arch guards I've made - similar application toyours and the stiffness or CF combined with the abrasion resistance of kevlar in a single cloth seemed like a really good combo.

Keep posting progress - great to see what others are doing!

Stuart
MaxiDave
MaxiDave
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 158
Hey Stuart,

I'm actually going to make 2 wings and front bumper from Carbon Kevlar for a bit

more strength, I will add extra patches/layers to the lower corners of the front

bumper and places like that where it will get hit hard.

Your a lucky man to have a Lotus Sunbeam.