MaxiDave
MaxiDave
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 14,
Visits: 158
Not sure if this is the correct section so please move if need be.
Up until last week I never even held a piece of carbon or kevlar cloth
until I undertook this massive project.
The plan is to make a complete wide arch bodykit for a 106 Maxi rally car and it had
to be kevlar as per the genuine Peugeot sport item.
I sourced a set of moulds, got all my material from Easy Composites and jumped in feet first.
I did it all hand lay up, 1 layer of 300g kevlar, 2 diolen and a final 300g kevlar.
I'm more than delighted with the results, a few dry spots but its going to be painted anyway so I can fill the low spots.
Reply
Like
2
Jack.Strong
Jack.Strong
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 549
Very Nice!!!!
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
looks good! is it stiff enough?
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
Leon
Leon
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 606
Hii..
That would be Looks great and cost effectiveness for painted product finish, kevlar is dificult enough to trim and cut.. realy great for abrasion purpose. What the resin you use for hand lay up this fabric?
Regards
Leon
Reply
Like
2
MaxiDave
MaxiDave
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 14,
Visits: 158
I was able to stand on the wing without doing any damage.
The quarter panels are a little more flexable so I might add some kevlar
square patches to the rear for more stiffness. I have already used 5-6 layers of kevlar
around the wheel arch area to add strength incase it rubs the wheel or is
lifted by the arch.
Reply
Like
2
stuart321
stuart321
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 37,
Visits: 178
Those panels looks great and really impressive given you have just started doing this - great find getting hold of the moulds!
Have you looked at the carbon/kevlar mixes? eg
Carbon/Twaron
I've got some of this sat waiting for some Lotus Sunbeam arch guards I've made - similar application toyours and the stiffness or CF combined with the abrasion resistance of kevlar in a single cloth seemed like a really good combo.
Keep posting progress - great to see what others are doing!
Stuart
Reply
Like
3
MaxiDave
MaxiDave
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 14,
Visits: 158
Hey Stuart,
I'm actually going to make 2 wings and front bumper from Carbon Kevlar for a bit
more strength, I will add extra patches/layers to the lower corners of the front
bumper and places like that where it will get hit hard.
Your a lucky man to have a Lotus Sunbeam.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search