By MaxiDave - 12/6/2012 9:14:22 PM

Not sure if this is the correct section so please move if need be.

Up until last week I never even held a piece of carbon or kevlar cloth

until I undertook this massive project.

The plan is to make a complete wide arch bodykit for a 106 Maxi rally car and it had

to be kevlar as per the genuine Peugeot sport item.

I sourced a set of moulds, got all my material from Easy Composites and jumped in feet first.

I did it all hand lay up, 1 layer of 300g kevlar, 2 diolen and a final 300g kevlar.

I'm more than delighted with the results, a few dry spots but its going to be painted anyway so I can fill the low spots.













By MaxiDave - 12/8/2012 6:28:01 PM

Hey Stuart,

I'm actually going to make 2 wings and front bumper from Carbon Kevlar for a bit

more strength, I will add extra patches/layers to the lower corners of the front

bumper and places like that where it will get hit hard.

Your a lucky man to have a Lotus Sunbeam.