+x beliblisk - 6/9/2020 11:24:29 AMWell OEM alu sits at 10.4kg.Top half weights 2.5kg and its 1mm thick. This bonnet is quite big as i just managed to get 1.5m cf cloth to fit OEM closing mechanisms will be used and with these you really need to push a bit on the hood (i imagine something much thinner would just warp to much). Ill post more pics (including guns ) once i try to correct "island"