Hi

I am building a table using scrap ply (bear withme, it will be better than it sounds.)

The table top is a 3/4 inch ply sheet cut to  random shape of approx 8ft x4ft with a central random shaped hole in the centre. (see the hasty sketch attached.)

My questions are , which product would be the best for this application and would it be sufficiently strong across this span at only 19mm thickness?




Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I would look at the GlassCast 50 Clear Epoxy Casting Resin.  In wood it can be cast up to 25mm per layer.

I would expect it to be pretty strong at that thickness.  You would need to prepare the wood edge with a nice rough key to help with adhesion.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search