Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Resin Casting and Moulding Forum
»
Clear Casting and Coating
»
River/Lake Table
River/Lake Table
Post Reply
Like
8
River/Lake Table
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Warren (Staff)
Warren (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
I would look at the
GlassCast 50 Clear Epoxy Casting Resin
. In wood it can be cast up to 25mm per layer.
I would expect it to be pretty strong at that thickness. You would need to prepare the wood edge with a nice rough key to help with adhesion.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
9
SimonW
S
SimonW
posted 6 Years Ago
ANSWER
HOT
Topic Details
S
Group: Forum Members
Posts: 1,
Visits: 5
Hi
I am building a table using scrap ply (bear withme, it will be better than it sounds.)
The table top is a 3/4 inch ply sheet cut to random shape of approx 8ft x4ft with a central random shaped hole in the centre. (see the hasty sketch attached.)
My questions are , which product would be the best for this application and would it be sufficiently strong across this span at only 19mm thickness?
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search