Hi I infused half of a hull this weekend and after it had infused I found the pressure started dropping my question is, can the vacuum pump be left on while the part is curing of will in suck the resin out the laminate or could in put and extra vac port in that doesn't come in to contact with the infusion mesh. Also does anyone know of and infusion mesh that is easy to use. 
Reply
Jcookson
Jcookson
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 5, Visits: 124
interesting but thre way i want to try is putting an extra vac point on the underside on the mould so no resin can be sucked through.