GC50 gel coat flaking off


Author
Message
Daz
Daz
Daz
posted 5 Years Ago HOT
Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Why is this happening .
I used pro finish carbon
Sprayed the mold with the gc50
Left over night to cure !!!
what can I do to rectify the delaminaton problem
Edited 5 Years Ago by Daz
Replies
Big Tee Racing
Big Tee Racing
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 6, Visits: 514
Morning , I've used GC50 before and had pre release problems , the only way I found to get over it was spraying a really dusty coat of gel coat in the mould , really dry and dusty . If applied in a normal way as to get a wet finish I would get the pre release
Hope this helps
Daz
Daz
Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)Supreme Being (688 reputation)
Group: Forum Members
Posts: 93, Visits: 651
This isn’t a pre release problem
It’s flaking off the bonnet
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Daz - 5 Years Ago
Big Tee Racing - 5 Years Ago
Daz - 5 Years Ago
Warren (Staff) - 5 Years Ago
Daz - 5 Years Ago
MarkMK - 5 Years Ago
Warren (Staff) - 5 Years Ago
Daz - 5 Years Ago
Warren (Staff) - 5 Years Ago