By Daz - 5/4/2020 4:24:47 PM
Why is this happening . I used pro finish carbon Sprayed the mold with the gc50 Left over night to cure !!! what can I do to rectify the delaminaton problem
|
By Warren (Staff) - 5/7/2020 10:08:33 AM
Round my way in the Midlands its about 10C at its coldest so if similar for you that won't have been ideal and may be a factor causing the delam.
|
|