Hello, at the moment I prefer to brush gelcoats or pattern coats as I don't have the proper equipment to spray.
Despite the quality of the brush and some thinning, I always end up with brush strokes so a lot of high and low spots.
What is your recommended tool to flatten out the brush strokes?
Besides manual sanding, I am looking into orbital and roto-orbital sanders but not sure what works best or if exist better tools for the job.
Any feedback would be greatly appreciated!
Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 4/26/2020 1:22:44 PM
Random orbital.

Thanks!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search