Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
2 tiny questions
2 tiny questions
Post Reply
Like
2
2 tiny questions
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Sharper
Sharper
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 35
I will soon be doing my 1st resin infusion project. I have a couple of small things to ask:
1: The shape I am making is rectangular, so would it be best for the resin to a) infuse from the short end, so it has further but narrower to go, or b) on the long ends, so it doesn't have as far to go but would have to spread out more?
2: I am slightly concerned that where the material is touching the front of the mould before infusion, resin won't get in between, giving it a nice finish (no fabric poking through). Is this a common problem? or does the resin always find a way to coat the the material?
Thanks for your help
(
|
|):::::::
o
: (||[[(
(
)))))))))))))))))))))))))))))))))))))))))))))))))))))))))))))
)
Reply
Like
2
Reply
fgayford
fgayford
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Infuse from the wide end. I once got caught trying to infuse a part that had a narrow section and the resin would just not make it all the way up that channel.
Fred
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
2 tiny questions
Sharper
-
13 Years Ago
Infuse from the wide end. I once got caught trying to infuse a part that had a narrow section and...
fgayford
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search