This is my first time using epoxy resin and I'm trying to make a Philips Hue Signe floor light.
The base is beech and so is the upright, for lighting I'm using the Philips Hue Lightstrip Plus.
After speaking to GlassCast® they have advised I use GlassCast® 50, I will also be adding White GlassCast Opaque Colour Pigment.
I’ve figured out all the mechanics to make this work and have the base made from a solid piece of Beech and the upright, however I need help with the resin pour.
I have attached a rough sketch and a photo in workshop showing test assembly, and hope it's clear what I am trying to do - see below.
The pour will be inside Clear Perspex Tube 36 x 30mm Bore x approx 1200mm long.
I will be cutting the cable from the controller unit and lightstrip and reconnecting through base then I will epoxy resin the base so seal in the controller.

Questions:
I will fix the led to the upright and slide the beech down the tube (beech upright is 30mm x 15mm), then I will close of the top and pour from the bottom.
1) Can I pour this in one go and if I do will it be full of bubbles.
2) Will I need to seal the surface of the beech upright before I pour.
3) I will remove the clear acrylic tube once set, will this be an issue – hard to remove, or could I use a release agent prior to casting.
4) White Colour Pigments, not sure on how many drops to make it opaque enough that the led light is bright and clear but you can’t see the lightstrip.
5) I've watched videos on pouring onto led lights but worried the heat from resin will melt the lightstrip cover, thoughts on this please.

Sorry for a lot of questions but want to make sure I don't mess this up as it's costing me a few pound to do this.
For now I think that covers it and in advance many thanks for your help, btw what do you think of this?
Many Thanks
Dave







Reply
David Grant
David Grant
Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)Supreme Being (196 reputation)
Group: Forum Members
Posts: 13, Visits: 86
Warren (Staff) - 4/14/2020 4:43:28 PM
2 pours will be safer but you should be able to do it in one with the relatively small volume.  It is always a bit hard to tell in these situations as wood can insulate the cast a lot and cause an exotherm.  Perhaps setting up a fan to blow over the resin filled tube once poured might help take some of the heat away.  

Yes we would recommend sealing wood in almost all cases.  Resin can soak in displacing air which can then get trapped as bubbles in your resin.

Use EasyLease or similar release agent on the tube.  At that length you will struggle to pull it off so you may need to very carefully slit the tube to "peel" it off the casting.

I would do a small experiment first to see how much pigment you need for the desired look.

The above advice with the fan may help keep the exotherm down a bit.  Typically I would expect to see around 60C during the cure - more if the exotherm begins to run away a bit.

Warren,
A great help you've been.
Regarding two pours, would that be possible as I couldn't check the ‘B-stage’ down the tube.
If I've calculated correctly then I should need about 540g of resin.
Happy to test pigment for desired look but would you advice I keep log of ratio of pigment drops to resin so I can match on main pour.

Dave



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
DaveGrant - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago
Warren (Staff) - 5 Years Ago
DaveGrant - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search