Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Swim platform advice needed
Swim platform advice needed
Post Reply
Like
1
Swim platform advice needed
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Massimiliano
M
Massimiliano
posted 5 Years Ago
ANSWER
Topic Details
M
Group: Forum Members
Posts: 167,
Visits: 1.1K
Hi, I am planning to replace the all metal swim platform on my boat with composites ones to save weight.
The current solution is as below from a project point of view, I am asking if it does make sense to build the "C" shaped support in fiberglass (as the rest of the swim platform) glued to the plane VS building it in SS and bolting it to the plane.
The tube connecting the transom and the swim platform is just for adding strength and load balancing and it is not intended to move or shake (even if some vibration can be forecasted).
Thanks
Reply
Like
1
Reply
Warren (Staff)
Warren (Staff)
posted 5 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Its about spreading the load. So you can use bond on fasteners with large bases, bond on the U shape bracket (as long as it has a reasonable surface area), fit load spreading inserts into the composite, metal plates etc.
As long as you avoid the point loading. Even large repair washers are better than a simple nut and bolt.
You can have extra reinforcement in that area to make a load spreading pad which the stainless bracket is bonded to. Something like our
VM100 Black 10min Methacrylate Adhesive
has good bonding properties to composite and stainless. Both surfaces need a rough key, rougher the better, and thorough clean and degrease.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Swim platform advice needed
mporta71
-
5 Years Ago
Make sense from what perspective? Cost? Weight saving? Ease of building? Strength? Could be a yes or a no depending on what your priorities are. Strength wise, mechanically fastening to composites i...
Hanaldo
-
5 Years Ago
Thank you Hanaldo! My goal is to save weight as much as possible but it has to be durable so the SS U-section seems the best compromise. Can you advise the best product to bond SS to fibreglass? An...
mporta71
-
5 Years Ago
Its about spreading the load. So you can use bond on fasteners with large bases, bond on the U shape bracket (as long as it has a reasonable surface area), fit load spreading inserts into the...
Warren (Staff)
-
5 Years Ago
Bang on Warren! I would bond the SS U-section. Faster, easier, stronger, not going to make a significant difference to weight. A methyl methacrylate like the VM100 Warren suggested would be my choic...
Hanaldo
-
5 Years Ago
Thank you both!!
mporta71
-
5 Years Ago
Post Reply
Like
1
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search