dubster
dubster
posted 4 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 15,
Visits: 126
Hello everyone,
I would like to cast the backplate of a tail light. silicone 2 piece mould is already made and I am looking for the right casting resin.
As this part is needed to mount on the car (screws), it must be strong / flexibility is not important. Needs to be UV resistant for years. on some places, part is only 2MM thick.
I was thinking to use the Xencast P6 resin, eventualy combined with carbon fibre powder (as the part must be black anyway).
Is this the best solution or are there other solutions / suggestions?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Tail light backplates
dubster
-
4 Years Ago
P6 with milled carbon fibre would certainly give a strong combination. You just need to be careful to mix it thoroughly and ensure there is no moisture in the moulds and its not too humid when you...
Warren (Staff)
-
4 Years Ago
thanks for your reply Warren, will post cure the resin. inside of the tail lights is paintend silver for reflection. perhaps there is a coating in the easy comp range that reflects (light and heat)?
dubster
-
4 Years Ago
We don't have any silvered coatings like that. I believe on most original parts it is a plastic chroming process. It might be worth looking in the vehicle restoration trade to see if there is a paint...
Warren (Staff)
-
4 Years Ago
Thanks for the advice, i will make an order today
dubster
-
4 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search