Hi, I'm currently restoring a trunk lid and my plan is to do a split mold as in EC hood-mould tutorial. I have one question though. 
As seen in the picture the outside skin is wrapped around the inside. I'm wonder if is is anything I have to think about with that edge ? I'm using wax on it to prevent mechanical lock. have anyone done something similar that can show a picture of their mould ?
Thanks for the help, Best regards Marcus 



Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You make it in the exact same manner that EC did with their bonnet tutorial. All 2-skin metal panels will be made with that crimped join, thats how they do it. If you have a look in the EC video, you will see they have the same crimp and can watch what they do with it. For composites, you will just end up with that lip on the inside skin, but it obviously wont wrap around from the outer skin anymore.
Edited 6 Years Ago by Hanaldo
Hansson43
H
Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)
Group: Forum Members
Posts: 23, Visits: 2.1K
Okey, thank you a lot Hanaldo!