Hi all,
I would like to confirm that I can use your green epoxy tooling gelcoat  on laminated moulds instead of the epoxy mould paste.
Thanks

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes the EG60 Epoxy tooling gel can be used in that way no problem, backed up with woven cloth (be it glass or carbon) and a good quality epoxy laminating resin.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant