By giantpt - 3/26/2020 10:11:39 AM
Hi all, I would like to confirm that I can use your green epoxy tooling gelcoat on laminated moulds instead of the epoxy mould paste. Thanks
|
By Warren (Staff) - 3/26/2020 1:29:07 PM
Yes the EG60 Epoxy tooling gel can be used in that way no problem, backed up with woven cloth (be it glass or carbon) and a good quality epoxy laminating resin.
|
|