	Group: AdministratorsPosts: 2.5K, 
    Visits: 8.5K
 
 | 
                    
			            Yes the EG60 Epoxy tooling gel can be used in that way no problem, backed up with woven cloth (be it glass or carbon) and a good quality epoxy laminating resin.                
			            
 Warren Penalver
 Easy Composites / Carbon Mods - Technical Support Assistant
 
 |