As Hanaldo eluded to, the surface would need to be sealed to stand any chance with a chemical release agent and most release agents. You might have some success with mould release wax as it can seal the pores, but realistically a sealed surface, be it 2 pack paint, or a coat of epoxy, would give you a much better surface and a good chance of release with pretty much any release agent.