By SHaas - 3/21/2020 6:28:23 PM
Hi everybody,
anyone has experience with Easy lease and platter? I sealed some places of the mould with platter and now I am wondering if I need to use release tape on top of the platter or if I have a chance with easy lease.
Thanks in advance
|
By Warren (Staff) - 3/23/2020 3:08:32 PM
As Hanaldo eluded to, the surface would need to be sealed to stand any chance with a chemical release agent and most release agents. You might have some success with mould release wax as it can seal the pores, but realistically a sealed surface, be it 2 pack paint, or a coat of epoxy, would give you a much better surface and a good chance of release with pretty much any release agent.
|
|