Best way to make fiberglass angles


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, I would like to make angles similar to the pre-preg ones on sale on the EC website, but in epoxy + fiberglass.
Thickness has to  be 5mm.
What is the best way to build the mould?


Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Warren (Staff) - 3/9/2020 4:20:01 PM
You could do it with an inner mould as well as a compression mould.  Clamp the moulds together with some wood as a load spreader and wind up the load.  That way when it's cured you will get a gloss finish on both sides of the angle. 

Thank you!


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search