+x mporta71 - 3/4/2020 4:58:33 PMHi, I would like to make angles similar to the pre-preg ones on sale on the EC website, but in epoxy + fiberglass.Thickness has to be 5mm.What is the best way to build the mould?
+x andrewt1971 - 3/5/2020 9:00:02 AM+x mporta71 - 3/4/2020 4:58:33 PMHi, I would like to make angles similar to the pre-preg ones on sale on the EC website, but in epoxy + fiberglass.Thickness has to be 5mm.What is the best way to build the mould?I would just buy a piece of aluminium angle that was large and rigid enough, polish it up and use that as the mould.