Hello, My name is Struan and I am an amateur motorcycle builder based in Scotland. I have a blog outlining all of my build process here www.remotorcycled.com for anyone interested.

On my newest build, I want to build a front light panel for the bike out of carbon fibre. I have designed the faceplate in CAD and I am now at a crossroads on how to turn this into a reality.



I was wondering whether I can get the part 3D printed and make a mould off this? The mould would really only need to be one-sided as the back of the light board wouldn't really be seen. I am going with this more for the visual impact than structural benefit (I will sort out the other issues that is LED's etc in time) but it would be good to get started with this. 

I am happy to invest time and money into this as there are other parts I quite fancy building also (wheel arches, panels etc).  As a complete beginner can you advise on the best method to do this? Am I better off going down the wet resin vacuum bag route or a prepreg route? My only concern with the prepreg is access to an oven which will allow me to function a vacuum pump. 

I am happy to consider anything really. I enjoyed working with fibreglass on my last build and I want to see what else I can learn.

thanks
Struan 

Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Typically you would want something like a 200gsm (or similar, eg 210gsm we sell) cloth for the surface layer and some backing reinforcement.  If it is supporting the weight of the LED lights, perhaps around a mm thick which would be 4 layers of a typical 200g cloth or less layers if you back up with a thicker cloth. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
remotorcycled
r
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 4, Visits: 17
Warren (Staff) - 2/18/2020 10:56:49 AM
Typically you would want something like a 200gsm (or similar, eg 210gsm we sell) cloth for the surface layer and some backing reinforcement.  If it is supporting the weight of the LED lights, perhaps around a mm thick which would be 4 layers of a typical 200g cloth or less layers if you back up with a thicker cloth. 

Thank you Warren, I will have a look on the Easy composites website and see what kits I can buy for this