+x mscomposites - 11/20/2019 2:30:32 PMThanks for the info MarkMK, Yes we do already give it a resin break, but one thing we are doing is clamping off the inlet line first and a minute later clamping off the exit. No resin is traveling down the exit line when we clamp. But I do notice that the small pits we are getting are in the inlet side. So i’m guessing it has to do with the bag being looser on that side? Or maybe since there’s more resin on that side at the time it gassed off differently and shows signs on the surface?