Does anyone know of any software or plugins for software that can take a 3D model and output the stencils for prepreg? I'm working with a complex shape and can't get my head around how to figure out all the little pieces and overlaps. Not to mention, figuring out how to repeat the process efficiently and accurately.

Thanks
Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Otolithco - 11/11/2019 7:26:59 PM
Does anyone know of any software or plugins for software that can take a 3D model and output the stencils for prepreg? I'm working with a complex shape and can't get my head around how to figure out all the little pieces and overlaps. Not to mention, figuring out how to repeat the process efficiently and accurately.

Thanks

Exactflat plugin for Fusion 360!