Group: Forum Members
Posts: 37,
Visits: 939
|
Hi guys, so I infused two parts, I used 650g on one part and 3x 200g on the other part. Both were infused on the same day, same temperature and demoulded at the same time, however the 650g part it came out extremely flexible almost like I could fold it up! The 3x 200g part is nice and solid
Am I missing something? Why did the 650g part come out so flexible
|