Having made about 8 medium sized carbon fibre parts now, I am less sure of release agent approach than when I started. I spent a year of part time plug making to build my most recent plug, coated it with 5 coats of easy-lease and on demoulding it destroyed the plug and severely damaged the mould. I have had one successful easy separation from a mould on the smallest of my parts and that was using meguiars wax x 10 coats.
Easy-lease just doesn't ever seem to work for me and when I've asked about problems with it I'm told it's got a shelf life (of what I don't know) and even in a sealed tin it goes off - bad news given the price it is and the lack of confidence that induces when using it!

What combinations/approaches can I use to get the best release when resin infusing using the uni-mould system and epoxy? Can I lay down some P120 sealer on the moul sand then add easy-lease on top or even PVA? If I look at Meguiars gold, PVA, P120 and easy-lease, what combinations give the best part release based on your experiences please? Grateful for any advice as this is a complex mould and I can't afford the time to go back to the start...
Replies
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
S120 will work in exactly the same way as the HP2002.
moonpie
moonpie
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 34, Visits: 94
[quote]
Rich (Staff) - 9/30/2019 1:54:17 PM
S120 will work in exactly the same way as the HP2002.

Thanks Rich - I have some of that now so will definitely try it first...what can I use on top of it though - wax, easy-lease, pva or just leave it as is?

Edited 6 Years Ago by moonpie
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
moonpie - 6 Years Ago
f1rob - 6 Years Ago
Hanaldo - 6 Years Ago
Fasta - 6 Years Ago
moonpie - 6 Years Ago
f1rob - 6 Years Ago
f1rob - 6 Years Ago
scottracing - 6 Years Ago
moonpie - 6 Years Ago
scottracing - 6 Years Ago
Rich (Staff) - 6 Years Ago
moonpie - 6 Years Ago
Rich (Staff) - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search