Bought this glasscast 3 for a project about 8 months ago and worked very well.
Mixed up a litre today by weight 100/50 as per instructions for 10 minutes. Steam started coming off and went totally solid a couple of minutes later....... really not happy !!!!!


Replies
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
80x26x0,3cm=0,62L. And 3mm is the Upper end. But that is not my point. You simply can not let epoxy stand around (or mix) in a compact 1L container. The reaction will build up heat, which accelerates the reaction, wich accelerates the heat production and so on. This can only be done with extra low reactivity resins like gc50.

Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
I see and I get what you’re saying however I followed the instructions correctly.
There should be limitations written on the instructions as to what not to do then if this is the case.
As far as I’m concerned, I followed the mixing instructions correctly but I appreciate what you’re saying so thank you 👍
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Bhamoggy - 6 Years Ago
Hanaldo - 6 Years Ago
Bhamoggy - 6 Years Ago
oekmont - 6 Years Ago
Bhamoggy - 6 Years Ago
oekmont - 6 Years Ago
Bhamoggy - 6 Years Ago
oekmont - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search