Group: Forum Members
Posts: 550,
Visits: 27K
|
80x26x0,3cm=0,62L. And 3mm is the Upper end. But that is not my point. You simply can not let epoxy stand around (or mix) in a compact 1L container. The reaction will build up heat, which accelerates the reaction, wich accelerates the heat production and so on. This can only be done with extra low reactivity resins like gc50.
|