I'm 3 months into my training as a laminator and I'm slowly acquiring the tools I need.

I have most of the tools that I'm able to buy - scalpels, snap blades, rulers etc.

I have just made myself a carbon fibre dibber for bagging, but I really need a PTFE dibber for the laying up process. However, the company I work for doesn't really use PTFE, so I'm struggling to get my hands on one.

If anyone has any spare that they can give me I would be so grateful!

Cheers
Steve
Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
YouStoleMyMash - 8/23/2019 6:10:44 AM
scottracing - 8/22/2019 10:14:56 PM
ive always made my own dibbers, the company that you are working for do they allow the use of PTFE dibbers as many aerospace companies don't?

You can make dibbers out of plastic or composites, for the tight corners i use a steel rule with the sharp corners taken off.
I would suggest you buy a  small sheet of PTFE and see if you can copy one of the other lammys dibbers. Have a look at my selection here.

http://www.talkcomposites.com/16604/RE-Lets-see-you-dibbers#32505

Hi, thanks for getting back to me. 

They do allow the use of PTFE dibbers. I had a look at buying a sheet last night, but was unsure about what size to get. Do you think 6mm thickness would be ok?

Also, how would you go about shaping it? I.e. What would you use to cut it and what would you use to make it smooth?

Cheers


bandsaw to cut the shapes out and then just normal sanding tools to do the sanding and contours, I spent a couple of hours doing mine.
Ask  the other laminators if you can see there dibbers Smile and ask if you can draw round them onto a template and transfer to the PTFE. Its also worthgetting some cured carbon sheet and making some from that or Tufnel.

YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
scottracing - 8/23/2019 8:46:51 PM
YouStoleMyMash - 8/23/2019 6:10:44 AM
scottracing - 8/22/2019 10:14:56 PM
ive always made my own dibbers, the company that you are working for do they allow the use of PTFE dibbers as many aerospace companies don't?

You can make dibbers out of plastic or composites, for the tight corners i use a steel rule with the sharp corners taken off.
I would suggest you buy a  small sheet of PTFE and see if you can copy one of the other lammys dibbers. Have a look at my selection here.

http://www.talkcomposites.com/16604/RE-Lets-see-you-dibbers#32505

Hi, thanks for getting back to me. 

They do allow the use of PTFE dibbers. I had a look at buying a sheet last night, but was unsure about what size to get. Do you think 6mm thickness would be ok?

Also, how would you go about shaping it? I.e. What would you use to cut it and what would you use to make it smooth?

Cheers


bandsaw to cut the shapes out and then just normal sanding tools to do the sanding and contours, I spent a couple of hours doing mine.
Ask  the other laminators if you can see there dibbers Smile and ask if you can draw round them onto a template and transfer to the PTFE. Its also worthgetting some cured carbon sheet and making some from that or Tufnel.

If u don't have access to a bandsaw would a coping saw, or something like that, do the trick? Is there a particular grit of sand paper you'd recommend using?

Cheers

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
YouStoleMyMash - 6 Years Ago
scottracing - 6 Years Ago
YouStoleMyMash - 6 Years Ago
scottracing - 6 Years Ago
YouStoleMyMash - 6 Years Ago
Rich (Staff) - 6 Years Ago
scottracing - 6 Years Ago
scottracing - 6 Years Ago
f1rob - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search