I'm 3 months into my training as a laminator and I'm slowly acquiring the tools I need.
I have most of the tools that I'm able to buy - scalpels, snap blades, rulers etc.
I have just made myself a carbon fibre dibber for bagging, but I really need a PTFE dibber for the laying up process. However, the company I work for doesn't really use PTFE, so I'm struggling to get my hands on one.
If anyone has any spare that they can give me I would be so grateful!