Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
It's a lot of fibre to take off, it would certainly affect the strength. Whether the thing has been engineered to calculated load tolerances is another matter, it's possible you could flatten that out and it would still be plenty strong. But it is also possible that it would make it too weak, so it's a risk.
I would at least try to talk to the guy, he may be reasonable.
|