Hello, i would like to do a fibreglass bonnet for my car and have a question. It's a simple shape with just 4 lines over the bonnet so i would like to build it on the original bonnet and use it (no mould)
I dont care much about the outer finish because it will be sanded and painted.

I checked the site and the only fabric wide enough is biaxial (i need 124cm width)

How much layers of 320g fabric would be enough for the part? I will make reinforcing strips on the underside and it will be mounted on the car with 4 hood pins.

I was thinking of using some 160g fabric for top layer but there is no 1.27m wide... 

What products would i have to purchase to make it?
Reply
Alanv6
Alanv6
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 22
Well first i have to buy some cloth from you Smile