Pump failed during an initial low-temp cure cycle using the XT135 Tooling prepreg.(400mm diameter x 22mm part size)
I have emptied out the oil and it is a dark brown colour.(no metal checked with a magnet) The pump is seized however the motor seams to want to turn.
Order the pump on 13/05/2019 and has been used three times.

Reply
flamano
flamano
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 10, Visits: 141
Warren (Staff) - 6/12/2019 10:38:41 AM
Sorry to hear your pump has failed. Sounds like something has majorly gone wrong with the pump for it to stop working like that.  As the pump is still under warranty we would recommend you return it to us and we will investigate for repair or replacement.

From your account details I cannot find your order, can you message me or email us on technical@easycomposites.co.uk with your order number and I will put a note on to expect your pump back for repair or replacement.  Also please put a note in the box so we know that the pump is yours.

Hopefully we can get this sorted for you quickly and get you back up and running.

Thank you for your reply,
My Order No #217329

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
flamano - 6 Years Ago
Warren (Staff) - 6 Years Ago
flamano - 6 Years Ago
Warren (Staff) - 6 Years Ago
flamano - 6 Years Ago
Warren (Staff) - 6 Years Ago
flamano - 6 Years Ago
Warren (Staff) - 6 Years Ago
Warren (Staff) - 6 Years Ago
flamano - 6 Years Ago
Warren (Staff) - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search