How strong is the 'High Strength Carbon Fibre Foam Core Panel 6mm'
How strong is the 'High Strength Carbon Fibre Foam Core Panel 6mm'
Post Reply
Like
6
How strong is the 'High Strength Carbon Fibre Foam Core Panel 6mm'
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
dazedproductions
dazedproductions
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 25
Don't seem to be any figures for it. Have made my own small cored panels but need something larger.
Will it hold a person over a span of 600mm?
Strong and rigid enough to be used as a table top with a span of 700mm?
Be interested to hear any subjective experiences of the cored panel that could help me understand.
Reply
Like
6
Hanaldo
Hanaldo
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Depends on the person, and how much deflection is tolerable, but should do both of those pretty easily in my experience.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search