By dazedproductions - 5/31/2019 6:16:12 PM
Don't seem to be any figures for it. Have made my own small cored panels but need something larger. Will it hold a person over a span of 600mm? Strong and rigid enough to be used as a table top with a span of 700mm?
Be interested to hear any subjective experiences of the cored panel that could help me understand.
|
By Hanaldo - 5/31/2019 10:03:15 PM
Depends on the person, and how much deflection is tolerable, but should do both of those pretty easily in my experience.
|
|