Hello there everyone. I bought a resin having the mixing ratio 100:2. I was wondering if using half I will use 50:1 or less 25:0,5 ? It is correct ?
Thank you !
Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
mdoru - 5/17/2019 10:21:04 AM
Hello there everyone. I bought a resin having the mixing ratio 100:2. I was wondering if using half I will use 50:1 or less 25:0,5 ? It is correct ? Thank you !

Sounds right.

Is it a polyester or vinyl ester catalyst?





mdoru
m
Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 162
It is polyester.