Group: Forum Members
Posts: 22,
Visits: 96
|
Thanks for all the useful advice!
I have a problem now because the buck is now painted with acrylic-nitro - I had read that Polyester on acrylic was ok but not the other way around. Can I use an epoxy on the acrylic paint? Hopefully I don’t need to strip all the paint off - that would be a job...
I will cover the steel with a pure epoxy coat before bonding it into the piece in a second epoxy carbon fibre hand lay operation.
Then I will join the front and back with epoxy adhesive.
Then I will make some holes and inject some 4 pound resin.
Thanks
|