I am using a MDF mould buck which I need to 'smooth' with primer and top coat of paint - I propose to use a nitro-acrylic paint - will that work with a gel coat and polyester resin which will be used to make the mould?

Thanks
By oekmont - 4/14/2019 2:00:29 PM

If you coat it, it would loose it's shine anyways. I had always had problems when using any 1k stuff, even when I used a 2k paint on top. Pva ruins your shiny surface, if you don't spray it very carefully. You could remove the acrylic with acetone and then coat the plug with whatever you want. That's just as much work as to coat the plug without removing the paint.