Hi, do you have any images of a cured part using the red poly/carbon twill please?

The red in my current fabric goes very dark once wetted and cured. I need something that maintains a bright red. I've found a fabric in the US but would be best not to import it.

Cheers
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
http://www.talkcomposites.com/Uploads/Images/27e8df90-5074-46e9-a65d-42c5.JPGhttp://www.talkcomposites.com/Uploads/Images/e53df685-9e7f-4e28-86f5-7f25.JPGhttp://www.talkcomposites.com/Uploads/Images/3b2c53db-4e94-4e9d-8fa9-8913.JPG

here's an example of red and black from a project i did a while ago, using resin infusion. if interested you can see the video on how it was made



Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search