What is the volume in litres of a 5kg pack of laminating resin? Thank you
Reply
Cedarcraft
C
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 2, Visits: 16
Warren (Staff) - 3/7/2019 10:36:59 AM
For simple estimation it is 5L by volume as the density is close to 1.

However to be precise the  density is 1.1 combined giving a more exact volume of 4.55L per 5kg.

Hi Warren thanks for that regards James 