Volume by weigh EL2 laminating resin

http://www.talkcomposites.com/Topic32268.aspx

By Cedarcraft - 3/7/2019 10:26:34 AM

What is the volume in litres of a 5kg pack of laminating resin? Thank you
By Cedarcraft - 3/7/2019 11:15:27 AM

Warren (Staff) - 3/7/2019 10:36:59 AM
For simple estimation it is 5L by volume as the density is close to 1.

However to be precise the  density is 1.1 combined giving a more exact volume of 4.55L per 5kg.