Omega
O
Omega
posted 7 Years Ago
ANSWER
HOT
Topic Details
O
Group: Forum Members
Posts: 3,
Visits: 56
Would there be any disadavantsges in using glasscast 10 to seal the edge of wood prior to using glasscast 50. This is to reduce the time between sealing and the main pour as the 10 is a faster cure resin. But I I don’t want this if adhesion or wood penitration is inferior.
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
No problem at all doing that. GlassCast 10 and 50 use the same resin just with different speed hardeners.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search