Hi all,
I have an original fibreglass part that I was intending to skin with carbon fibre but after a few disappointing and frustrating attempts I have now been toying with the idea of making a mould from the original part and using the infusion method to replicate the part in carbon fibre instead!!...  Obviously I will need to make a reverse mould!!.... but what materials do I need?? I'm not talking about the infusion/bagging side, just the moulding materials, methods and techniques to produce the mould itself??
Thanks
Pete.
Reply
Peter Robinson
P
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 7, Visits: 65
Warren (Staff) - 2/12/2019 9:29:20 AM
MarkMk is right about the Uni-Mould system.  The good thing is being based on a vinylester gelcoat, it is compatible with polyester and epoxy resins meaning that you could make a range of different finish and quality of parts from the same mould.

I will do a little more research into the Uni-mould system and check out some more of EC's tutorials on this, thank you for taking the time to reply.