+x Warren (Staff) - 2/12/2019 9:29:20 AMMarkMk is right about the Uni-Mould system. The good thing is being based on a vinylester gelcoat, it is compatible with polyester and epoxy resins meaning that you could make a range of different finish and quality of parts from the same mould.