Resin Infusion Problems - dry patches


Author
Message
Balakrishnan Seeni
Balakrishnan Seeni
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 5
Dear sir,

I did resin infusion process for 175 x 150 mm flat plate in glass and carbon fabric. But I faced huge problem. Here i attached the photos. Kindly help me to solve this problem.

I used Vacuum pump, specification is  630 mm of Hg (or )  24 in Hg. and its dry vacuum pump single stage. Is sufficient to do the infusion process?

Some times plate get good finishing. Some times problem will come (See the photos)
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Balakrishnan Seeni - 2/8/2019 10:43:26 AM
Dear sir,

I did resin infusion process for 175 x 150 mm flat plate in glass and carbon fabric. But I faced huge problem. Here i attached the photos. Kindly help me to solve this problem.

I used Vacuum pump, specification is  630 mm of Hg (or )  24 in Hg. and its dry vacuum pump single stage. Is sufficient to do the infusion process?

Some times plate get good finishing. Some times problem will come (See the photos)

Looks like you demoulded to early to me... you're talking of the problems on the bottom of your plate right? looks like resin was still sticking to the mould? You are using epoxy right? make sure it's fully cured at 25°C preferably even with a postcure and make sure to wait 48 hours to be sure before demoulding 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search