+x Balakrishnan Seeni - 3/3/2019 2:00:02 PM+x Lester Populaire - 2/8/2019 11:34:43 AMTo me this does not look like a pump/vacuum issue, but rather something that can be solved with the right infusion setup. Can you provide a picture of the opposite side of the part with the flow media?It might already be enough to just heat the vacuum bag with a heat gun along the sides, so it can conform better to the edge of the fabric to avoid race tracking.cheers, LesterThank You for valuable reply Lester.. here i attached the opposite side of the part. This side is fully impregnated. help me to solve the above problem
+x Lester Populaire - 2/8/2019 11:34:43 AMTo me this does not look like a pump/vacuum issue, but rather something that can be solved with the right infusion setup. Can you provide a picture of the opposite side of the part with the flow media?It might already be enough to just heat the vacuum bag with a heat gun along the sides, so it can conform better to the edge of the fabric to avoid race tracking.cheers, Lester