XE and RE 600 are not fabrics I am familiar with.
If either is a Unidirectional cloth then that would likely explain why it does not infuse as there are insufficient gaps in the cloth for resin flow..
Other things can cause problems like insufficient flow mesh, too thick resin, layout of resin feed and vacuum port etc.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|